Construction Materials Testing · Construction

Glass Impact Test

EN 12600 (glass in building — pendulum test, impact test method and classification)EN 12150 (thermally toughened soda lime silicate safety glass)EN 14449 (laminated glass — evaluation of conformity)EN 1863 (heat strengthened soda lime silicate glass)
Construction Materials Testing laboratory work

What Is Glass Impact Test?

In the EN 12600 test, a pendulum made of a double tyre is swung to strike a vertically mounted glass sample from defined drop heights. Assessment looks not only at whether the glass breaks but at the FRACTURE MODE: did the glass break safely, or did it produce large cutting shards?

Purpose of Glass Impact Test

The purpose is to determine whether the glass limits injury risk in the event of human impact. This classification is mandatory for glass in accessible locations such as doors, facades and balustrades.

Which Products Is Glass Impact Test Applied To?

  • Tempered safety glass
  • Laminated glass
  • Glass doors and partitions
  • Glass balustrades and balcony glazing
  • Facade and shop-window glazing

In Which Sectors Is Glass Impact Test Used?

ConstructionConstructionCementPublic SectorInfrastructure

Standards Related to Glass Impact Test

  • EN 12600 (glass in building — pendulum test, impact test method and classification)
  • EN 12150 (thermally toughened soda lime silicate safety glass)
  • EN 14449 (laminated glass — evaluation of conformity)
  • EN 1863 (heat strengthened soda lime silicate glass)

Glass Impact Test Conditions

impact device
Standard pendulum consisting of two rubber bags
Drop height
From standard according to classification levels
Specimen
Glass of standard size, fixed to the frame
Assessment
Non-breakage or safe breakage method

Equipment for Glass Impact Test

  • EN 12600 pendulum impact setup and test frame
  • Height adjustment and release mechanism
  • Post-fracture fragment assessment setup
  • High-speed camera (optional)

Sample Requirements for Glass Impact Test

  • The sample must be taken so as to represent the batch and in accordance with the sampling rules of the relevant standard.
  • The sampling date, location and the person who took the sample must be recorded.
  • Samples requiring curing or conditioning must be stored under the defined conditions.
  • The number of samples must meet the minimum required by the standard.
  • The sample must not be damaged during transport.

Duration of Glass Impact Test

A single sample's test is brief; the study can take a few days given the number of samples and height steps needed for classification.

Glass Impact Test Procedure

  1. 1The sample is fixed in the standard test frame.
  2. 2The pendulum is set to the height corresponding to the classification step.
  3. 3The pendulum is released and strikes the sample.
  4. 4If the sample did not break, the next higher step is used.
  5. 5When breakage occurs, the fragment structure is examined.
  6. 6The fracture mode is compared against the types defined in the standard.
  7. 7The classification code is determined and reported.

Glass Impact Test Acceptance Criteria

The acceptance class does not come from the test method but from the product standard and the project: concrete class, reinforcement class, aggregate category, or fire performance class is defined in the specification. The report gives the measured value; the conformity decision is made against the relevant product standard.

Evaluation of Results

Classification is made by jointly assessing the drop height the glass withstands without breaking and the fracture mode. Which class is required comes from the construction regulation and project specification according to the glass's location in the building.

Glass Impact Test Report

  • Sample description, sampling location and date
  • Sampling method and witness sample information, if any
  • Standard and test conditions applied
  • Sample dimensions, curing conditions and age information
  • Measured values and calculated results
  • Failure mode or damage description (where applicable)
  • A statement that the result applies only to the specimen submitted for testing

Accreditation

EUROLAB holds internationally recognised accreditation obtained from accreditation bodies party to the IAF and ILAC multilateral recognition arrangements, under ISO/IEC 17025 for laboratory testing, ISO/IEC 17020 for inspection and surveillance, and ISO/IEC 17021-1 and ISO/IEC 17065 for system and product certification. This chain ensures the reports and certificates issued are accepted worldwide.

Whether this test can be offered within accredited scope depends on your product and the standard applied; since accreditation is method-based, the scope is confirmed in writing at the quotation stage.

Scope and authorisations

Related Regulations

  • EU 305/2011 Construction Products Regulation (CPR)
  • Construction Products Regulation (Turkey)
  • TS 500 / Requirements for Design and Construction of Reinforced Concrete Structures
  • Turkish Building Earthquake Code

Construction Materials Testing — What Does This Testing Field Cover?

The section below describes the field that the Glass Impact Test test belongs to; the conditions and acceptance criteria of this particular test are given in the sections above. The scope specific to your product is confirmed in writing at the quotation stage.

Construction materials testing shows whether a product performs the function it takes on within the structure. A wide field is gathered in this family, from the compressive strength of concrete to the thermal transmittance of glass, from sieve analysis of aggregate to the watertightness of windows.

What sets this family apart from the others is that the result turns directly into a REGULATORY DECLARATION. For products covered by construction products legislation a declaration of performance (DoP) is mandatory, and every essential characteristic in the declaration rests on a test result. Reaction-to-fire class, thermal conductivity, compressive strength, water permeability and release of dangerous substances are declared in this way. The declaration is a legal text carrying the manufacturer's signature; the test record behind it is the first document requested in an inspection.

The second distinguishing feature is that the product is assessed over its SERVICE LIFE. An electronic device runs for five years; a building component stays in place for fifty and is exposed throughout that time to freeze-thaw cycles, UV, moisture, chemical attack and load. Durability tests (freeze-thaw, carbonation, alkali-silica reaction, ageing) therefore carry as much weight in this field as classical strength tests.

Tests are separated by material type and each group has its own set of standards: cement and concrete, aggregate, masonry units, wood-based panels, thermal insulation, glass and glazing units, ceramic tiles, floor coverings, screeds, joint fillers and coating systems. Where the product will be installed determines which set applies — the same panel is assessed against different standards on a wall and on a floor.

Factory production control (FPC) is a continuous component of the field. CE marking on a construction product is not obtained with a single test and then left; the manufacturer must set up a system showing that it monitors production consistency, takes samples regularly and intervenes when there is a deviation. Depending on the product group, this system may have to be audited by a notified body.

Site testing is a separate body of work. In the laboratory the product is approved; on site it is checked that the product really is of the declared class and that it has been applied correctly. Fresh concrete slump, cylinder sampling, aggregate sieve analysis and in-situ watertightness tests fall within this scope.

Method groups in this field

  • Concrete and cement

    Slump, air content and unit weight in fresh concrete; compressive and flexural strength, water permeability and freeze-thaw resistance in hardened concrete. For cement, compressive strength, setting time and composition analysis.

  • Aggregate

    Sieve analysis, particle shape, Los Angeles abrasion resistance, freeze-thaw, alkali reactivity and density/water absorption.

  • Thermal and energy performance

    Thermal conductivity and thermal resistance, calculation of thermal transmittance (U value) in glazing units, solar energy transmittance.

  • Facade and joinery

    Air permeability, watertightness and wind load resistance in windows and doors; fire performance in facade systems.

  • Fire performance

    Reaction-to-fire classification and fire resistance tests; these are two separate concepts and are addressed by separate standards.

  • Masonry, tile and flooring

    Compressive strength, water absorption, abrasion resistance, slip resistance, stain and chemical resistance.

  • Emissions and dangerous substances

    Formaldehyde release from wood-based panels, VOC emissions from construction products, leaching behaviour of aggregates and waste.

Commonly confused in this field

  • REACTION to fire and RESISTANCE to fire are different concepts: one describes the material's contribution to a fire, the other how long a component holds the fire back.
  • A declaration of performance is not a certificate; it is the manufacturer's declaration. Notified body involvement varies with the product group and the assessment system.
  • A test result is valid for the mounting arrangement in which the product was tested. A different substrate, a different thickness or a different joint detail may require reassessment.
  • A site sample and a laboratory sample are not the same thing. A concrete cylinder taken on site also reflects application and curing conditions; it does not replace product approval.
  • ASTM and EN construction standards measure similar quantities with different specimens and scales; the results cannot be converted one-to-one.

Which decisions these results support

  • Declaration of performance (DoP) and CE marking
  • Establishing and maintaining the factory production control system
  • On-site conformity control of concrete, aggregate and workmanship
  • Meeting fire and energy performance requirements
  • Verifying the technical items in the project and tender specification

Related Tests

Frequently Asked Questions About Glass Impact Test

Is tempered glass always safe?

Tempering ensures small, blunt fragments form on breakage, but classification is still demonstrated by test. The project determines which class the application requires.

Why does laminated glass behave differently?

In laminated glass, broken fragments remain adhered to the interlayer. Laminated glass therefore often achieves a higher class and is preferred in locations with a fall risk.